Mike, Thank you for the Link that is one good resource!
just about as good as MIL-DTL-16232G & I went to our local Naval plating plant and obtained their local engineered procedure.
Funny guys here are talking about phosphating bolts, when I was under the impression most "hardware" was post mfr. treated via a Black Oxide Coating for ferrous alloys which is a different process than photsphating.
just a suggestion a Alkaline Rinse (W hot & cold water rinse) would be a recommended PARTS activation after your denatured alcohol degreasing, just a thought,,,,
JIM